Copper Alloys: Choosing by Conductivity, Not by Strength

Steel is selected by strength and then adjusted for corrosion. Copper is selected the other way round. Almost every copper part exists because of what it conducts, and the entire alloy family is organised around a single question: how much conductivity are you willing to give up, and what are you buying with it?

Once that question is in place, the families stop being a list to memorise. Pure copper gives up almost nothing and gains almost nothing. Brass gives up most of its conductivity and gains machinability and cost. Beryllium copper gives up a lot and gains strength and elasticity. Cupronickel gives up most of it and gains seawater resistance. Every grade sits somewhere on that line.

Why Conductivity Is the Selection Axis

Conductivity in copper alloys is expressed as a percentage of the International Annealed Copper Standard, or IACS. The standard defines fully annealed high-purity copper at 20 °C as 100% IACS, and every commercial alloy is measured against that reference. The number is a comparison, not a material property in itself, which is why a higher figure is always better for electrical work and always costs something in mechanical properties.

Two consequences follow and they cause most of the confusion in copper specifications. First, conductivity and strength trade against each other almost linearly, because the alloying additions and the cold work that raise strength both scatter electrons. Second, conductivity is affected by temper as well as composition — the same grade in the annealed and hard conditions will not give the same reading, so a conductivity requirement without a temper requirement is incomplete.

What Each Alloying Element Costs

ElementBuysCostsFound in
Zn — zincStrength, machinability, lower material costLarge drop in conductivity, to roughly a fifth of pure copperAll brasses
Sn — tinElasticity, wear resistance, corrosion resistanceConductivity falls to roughly a tenth to a fifthPhosphor bronzes
Al — aluminiumStrength, wear resistance, corrosion resistanceConductivity falls sharplyAluminium bronzes
Ni — nickelSeawater and erosion-corrosion resistanceConductivity falls to a small fraction; cost risesCupronickels
Pb — leadMachinability; acts as a chip breakerRegulatory exposure in drinking water and RoHS contextsFree-machining brass
Be — berylliumVery high strength and elastic limit after ageingConductivity falls to about a fifth; dust hazard during machiningBeryllium copper
Cr, Zr — chromium, zirconiumStrength retained at temperature; resistance to softeningModerate conductivity loss, typically 15–25%Chromium copper, CuCrZr

Coppers: T2, TU1 and TU2, TP1 and TP2, TAg0.1

The unalloyed coppers are where the conductivity is, and the difference between them is not purity in the abstract but oxygen.

  • T1 and T2 (含氧紫铜, oxygen-bearing tough pitch copper) — copper plus silver of at least 99.95% and 99.90% respectively, with oxygen around 0.02–0.05%. Conductivity is essentially 100% IACS. This is the default for busbars, windings, current-carrying studs and large conductors: good conductivity, good formability, lowest cost of the family. The limitation is the oxygen. Copper containing oxygen forms a copper–copper oxide eutectic that melts around 1065 °C, and in a hydrogen-bearing atmosphere at brazing or welding temperature the oxide reacts and steam forms along the grain boundaries. That is hydrogen embrittlement, and it shows up as cracks in the heat-affected zone rather than as a defect you can see before brazing.
  • TU1 and TU2 (无氧铜, oxygen-free copper) — oxygen capped at 0.001% and 0.003%. Conductivity is at or marginally above 100% IACS. The absence of oxide removes the hydrogen embrittlement mechanism entirely, which makes these grades the right choice for vacuum components, brazed assemblies, electron tubes and any part that will see a reducing atmosphere at temperature. They cost slightly more and they are not improved for machining.
  • TP1 and TP2 (磷脱氧铜, phosphorus-deoxidised copper, DHP) — oxygen is removed during melting with phosphorus, leaving a residual of roughly 0.012–0.040%. Conductivity drops to about 97–99% IACS, which is a small price for a grade that welds and brazes cleanly and does not suffer hydrogen embrittlement. This is the standard choice for tubing, heat exchangers and any fabricated assembly where welded joints are unavoidable.
  • TAg0.1 (silver-bearing copper) — a small silver addition leaves conductivity close to pure copper while raising the temperature at which the material softens. It is chosen where a conductor runs hot and creep or annealing of the copper would be a problem, not where the conductivity figure itself is the constraint.

The selection rule is short: for plain current-carrying parts, T2. For vacuum, hydrogen or critical brazing, TU. For welded and brazed assemblies where a slight conductivity loss is acceptable, TP.

Conductivity by Family

These are typical ranges for commonly available grades, and they are the numbers that make the trade visible.

FamilyTypical conductivity (% IACS)What you get for the loss
T2, tough pitch copper~100Reference conductivity; low strength
TU1, TU2, oxygen-free100–101Same conductivity, no hydrogen embrittlement
TP1, TP2, deoxidised97–99Weldability and brazing reliability
Tellurium copper (C14500), sulphur copper (C14700)85–95Free-machining behaviour with conductivity far above brass
CuCrZr, chromium copper75–85Strength and resistance to softening at temperature
CuFe2P (C19400)~60Strength for lead frames and terminals
CuNiSi types45–60Elasticity and stress relaxation resistance for contacts
Brass H62, H5920–30Machinability, formability and low cost
Beryllium copper QBe218–22Very high strength and elastic limit
Phosphor bronze QSn6.5-0.110–20Elasticity, wear resistance and corrosion resistance

High-Copper Alloys: Strength Without Losing Everything

These grades keep the copper matrix largely intact and add small amounts of an element that precipitates on ageing. The result is a family that sits between pure copper and brass.

  • TBe2 / QBe2 (beryllium copper, C17200) — the highest strength available in a copper alloy, with an elastic limit that makes it the standard for repeated-cycle springs, relay blades and connector contacts. It is age hardened after machining, which means the part can be cut in the soft state and then brought to strength with minimal distortion. Two things belong on the drawing: the ageing condition, because it determines the strength, and the machining precaution, because beryllium-bearing dust is a health hazard and requires dust control and extraction rather than ordinary housekeeping.
  • TCr and CuCrZr (chromium copper, C18150 / C18200) — conductivity around 75–85% IACS with strength that survives elevated temperature. The property that matters is resistance to softening: a resistance-welding electrode has to stay hard while conducting and while being cycled thermally, which is exactly the combination these grades provide. They are also used for mould thermal-management inserts and contact bases.

Brass: Machinable, Cheap, Low Conductivity

Brass is copper with zinc, and at 20–30% IACS it is not a conductor in the electrical sense. It is chosen for machinability, formability, corrosion resistance in benign environments and cost: H62 for good cold formability, H59 for lower cost and higher strength, HPb59-1 as the free-machining grade that most turned fittings are made from.

The lead in the free-machining grades is deliberate and it is also the regulatory exposure. Lead-bearing brass is restricted in drinking water applications and has been progressively narrowed under RoHS, so a fitting destined for potable water needs the alloy confirmed against the applicable rule rather than inherited from an older drawing. Brass grades, their European and American equivalents and their machining behaviour are covered on the brass CNC turned fittings page.

Bronze: Wear and Elasticity

  • QSn6.5-0.1 (phosphor bronze, CuSn6 / C51900) — tin and a small phosphorus addition. Good elasticity, wear resistance and corrosion resistance at 10–20% IACS. The standard choice for spring contacts, wear shims, bearing bushes and precision instrument parts where both electrical conduction and mechanical elasticity are required.
  • QAl9-4-4 (aluminium bronze) — high strength, good wear resistance and good corrosion resistance, used for heavily loaded bushes, worm wheels, valve parts and wear-resistant structural components. There is no exact European equivalent; CuAl10Fe3 is the usual comparison and the mechanical properties should be checked rather than assumed.

Cupronickel: Seawater Service

  • B30 (70/30 cupronickel, CuNi30Mn1Fe / C71500) — high nickel content for corrosion resistance in seawater, used for condenser and heat exchanger tubing and marine structural parts. The cost is high and the conductivity is low, but nothing else in the family survives continuous seawater as well.
  • BFe10-1-1 (90/10 cupronickel with iron and manganese, CuNi10Fe1Mn / C70600) — the iron addition is the point. In flowing seawater, 90/10 cupronickel with iron resists erosion-corrosion substantially better than the plain alloy, because the iron modifies the protective film. For a seawater piping or heat exchanger application the iron content is a functional requirement, not a residual.

Equivalents

GB designationCommon EN / UNSNotes
T2C11000 (ETP copper)Oxygen-bearing; not for hydrogen-atmosphere brazing
TU1, TU2C10200 (OF copper)Oxygen-free; vacuum and brazed assemblies
TP2C12200 (DHP copper)Phosphorus-deoxidised; welded assemblies and tubing
C14500C14500 (tellurium copper)Free-machining, high-conductivity electrical parts
QBe2 / TBe2CuBe2 / C17200Age hardened; dust control required in machining
CuCrZrC18150Welding electrodes and thermal inserts
QSn6.5-0.1CuSn6 / C51900Phosphor bronze for springs and bushes
B30CuNi30Mn1Fe / C7150070/30 cupronickel, seawater
BFe10-1-1CuNi10Fe1Mn / C7060090/10 with iron, flowing seawater

What to Put in an RFQ

  • The grade, and the conductivity requirement if the part carries current — as a percentage of IACS, with the temper it applies to.
  • The temper: annealed, half hard, hard or aged. Conductivity, strength and machinability all depend on it.
  • Whether the part will be brazed, welded or used in a vacuum or hydrogen atmosphere, which decides between T2, TP and TU far more reliably than price does.
  • The service medium, particularly whether seawater, potable water or food contact is involved, because that constrains both the alloy and the lead content.
  • Any requirement for the alloy certificate, especially on grades where a substitution is difficult to detect visually.
  • Surface finish expectations, since copper alloys tarnish and the finish is often a functional requirement rather than a cosmetic one.

Frequently Asked Questions

Why did a T2 copper part crack after brazing?

Hydrogen embrittlement. Tough pitch copper contains oxygen as copper oxide, and at brazing temperature in a reducing or hydrogen-bearing atmosphere the oxide reacts and forms steam along the grain boundaries, which opens the metal from the inside. The crack appears in or next to the joint after the heat cycle. The remedy is a deoxidised or oxygen-free grade — TP2 for welded and brazed assemblies, TU1 or TU2 for vacuum and hydrogen service.

Can brass be used for current-carrying parts?

Only for low currents and short conduction paths. Brass runs at roughly 20–30% of pure copper's conductivity, so a brass conductor either carries far less current or runs far hotter than a copper one of the same size. Where brass appears in an electrical assembly it is usually a terminal body or a mechanical support and the current is carried by a copper contact, not by the brass.

Is CuCrZr a replacement for beryllium copper?

For some applications and not others. CuCrZr gives 75–85% IACS against roughly 20% for QBe2, and it holds hardness at higher temperature, which makes it better for welding electrodes and thermal parts. QBe2 reaches considerably higher strength and elasticity, which is what repeated-cycle springs and contact blades need. The substitution works where the requirement is conductivity plus thermal stability and fails where the requirement is elastic limit.

Need a Copper Alloy Component Machined?

DXSCNC machines drawing-based copper and brass components: threaded fittings, adapters, sleeves, contact parts and flanged bodies, in the temper and finish the drawing specifies.

Use the model-specific machining limits when planning a part. Material, geometry, tolerance, workholding and inspection affect machine selection.

Related DXSCNC resources: Brass CNC Turned Fittings, Plating on Copper Alloys, Threaded components and Valve and Fluid Control Applications.

Request a Quote for Copper Alloy Machined Parts